Polyethylene compositions and closures for bottles
US-9221966-B2 · Dec 29, 2015 · US
US10040634B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10040634-B2 |
| Application number | US-201515329242-A |
| Country | US |
| Kind code | B2 |
| Filing date | Jul 16, 2015 |
| Priority date | Jul 25, 2014 |
| Publication date | Aug 7, 2018 |
| Grant date | Aug 7, 2018 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
A rubber composition for heat-resistant conveyor belts contains an ethylene-1-butene copolymer having a Mooney viscosity at 125° C. of 20 or greater, and an ethylene-propylene copolymer having a Mooney viscosity at 125° C. of 20 or greater and an ethylene content of 40 to 60 mass %, and the mass ratio of the ethylene-1-butene copolymer to the ethylene-propylene copolymer is 10/90 to 90/10.
Opening claim text (preview).
The invention claimed is: 1. A rubber composition for heat-resistant conveyor belts comprising: an ethylene-1-butene copolymer having a Mooney viscosity at 125° C. of 20 or greater; and an ethylene-propylene copolymer having a Mooney viscosity at 125° C. of 20 or greater and an ethylene content of 40 to 55 mass %, wherein a mass ratio of the ethylene-1-butene copolymer to the ethylene-propylene copolymer is 10/90 to 90/10. 2. The rubber composition for heat-resistant conveyor belts according to claim 1 , wherein a Mooney viscosity at 125° C. of the ethylene-1-butene copolymer is 30 or greater. 3. The rubber composition for heat-resistant conveyor belts according to claim 1 , wherein an ethylene content of the ethylene-propylene copolymer is 40 mass % or greater and less than 60 mass %. 4. The rubber composition for heat-resistant conveyor belts according to claim 1 , further comprising an organic peroxide, wherein a content of the organic peroxide is from 0.011 to 0.020 molar equivalents relative to 100 parts by mass of the total of the ethylene-1-butene copolymer and the ethylene-propylene copolymer. 5. A heat-resistant conveyor belt comprising the rubber composition for heat-resistant conveyor belts according to claim 1 . 6. The rubber composition for heat-resistant conveyor belts according to claim 2 , wherein an ethylene content of the ethylene-propylene copolymer is 40 mass % or greater and less than 60 mass %. 7. The rubber composition for heat-resistant conveyor belts according to claim 6 , further comprising an organic peroxide, wherein a content of the organic peroxide is from 0.011 to 0.020 molar equivalents relative to 100 parts by mass of the total of the ethylene-1-butene copolymer and the ethylene-propylene copolymer. 8. The rubber composition for heat-resistant conveyor belts according to claim 2 , further comprising an organic peroxide, wherein a content of the organic peroxide is from 0.011 to 0.020 molar equivalents relative to 100 parts by mass of the total of the ethylene-1-butene copolymer and the ethylene-propylene copolymer. 9. The rubber composition for heat-resistant conveyor belts according to claim 3 , further comprising an organic peroxide, wherein a content of the organic peroxide is from 0.011 to 0.020 molar equivalents relative to 100 parts by mass of the total of the ethylene-1-butene copolymer and the ethylene-propylene copolymer.