Shrink wrap label coating to facilitate recycling
US-2018247570-A1 · Aug 30, 2018 · US
US10023359B2 · US · B2
| Field | Value |
|---|---|
| Publication number | US-10023359-B2 |
| Application number | US-201414900319-A |
| Country | US |
| Kind code | B2 |
| Filing date | Dec 22, 2014 |
| Priority date | Dec 22, 2014 |
| Publication date | Jul 17, 2018 |
| Grant date | Jul 17, 2018 |
A practical reading order for non-experts. Skip the full description unless you need deep technical detail.
What the patent document calls the invention.
A short plain-language summary of the technical disclosure.
Who owns or filed the patent and who is credited as inventor.
Filing, priority, publication, and grant dates set the timeline.
The legal scope of protection — read this for what is actually claimed.
Technology tags used to group this patent with similar filings.
Prior art links and similar publications in this corpus.
Official abstract text for this publication.
The invention relates to a shrink label. According to an embodiment the shrink label comprises an uniaxially oriented multilayer face film comprising skin layers including polyethylene polymer(s) and at least two cyclic polymers comprising different glass transition temperatures between 30 and 100° C. and the difference between the glass transition temperatures being between 5 and 60° C., and wherein the multilayer face film is seamed by a solvent. The invention further relates to a method for providing a shrink label, use of the shrink label, method for providing a shrink label and method for labelling.
Opening claim text (preview).
The invention claimed is: 1. A shrink label capable to shrink under exposure to external energy, the shrink label comprising: an uniaxially oriented multilayer face film including a first skin layer forming an uppermost layer of the face film and a second skin layer forming an undermost layer of the face film, wherein said skin layers comprise: at least one of the following polyethylene polymers: low density polyethylene, medium density polyethylene and linear low density polyethylene; at least two cyclic polymers, wherein the at least two cyclic polymers are cyclic olefin copolymers of norbornene and ethene, and wherein the at least two cyclic polymers comprise different glass transition temperatures between 30 and 100° C. and the difference between the glass transition temperatures is between 5 and 60° C.; and wherein the multilayer face film is turned over itself so that opposite edges of the multilayer face film are overlapping and forming an area wherein the first skin layer and the second skin layer are adjacent to each other and bonded together by a solvent so as to form a seam for the shrink label. 2. A shrink label according to claim 1 , wherein the at least two cyclic polymers comprises one cyclic polymer having the glass transition temperature below 70° C. and another cyclic polymer having the glass transition temperature above 70° C. 3. A shrink label according to claim 1 , wherein the at least two cyclic polymers comprise one cyclic polymer and another cyclic polymer, wherein an amount of the one cyclic copolymer is between 44 and 77 wt. % based on the total weight of the skin layer and an amount of the another cyclic copolymer is between 10 and 44 wt. % based on the total weight of the skin layer. 4. A shrink label according to claim 1 , wherein an amount of polyethylene polymer(s) is between 5 and 20 wt. % based on the total weight of the skin layer. 5. A shrink label according to claim 1 , wherein the polyethylene polymer is one of the following: copolymer of ethylene and 1-octene, and copolymer of ethylene and hexene. 6. A shrink label according to claim 1 , wherein the solvent is one of the following: alpha-pinene, limonene, mixture of tetrahydrofuran and 1,3-dioxolene, o-chlorotoluene, 4-chlorotoluene, and p-chlorobenzotrifluoride. 7. A shrink label according to claim 1 , wherein the uniaxially oriented multilayer face film comprises an orientation ratio of at least 3. 8. A shrink label according to claim 1 , wherein the multilayer face film is uniaxially oriented in a transverse direction and the transverse direction extends around a circumference of the shrink label. 9. A shrink label according to claim 1 , wherein the multilayer film is capable to shrink in a uniaxial orientation direction of the face film between 20 and 75% at a temperature between 65 and 98° C. 10. A shrink label according to claim 1 , wherein the multilayer face film has a three layer structure further comprising a core layer between the first skin layer and the second skin layer.
Recycling of unreacted starting or intermediate materials · CPC title
to be fastened or secured by the material of the label itself, e.g. by thermo-adhesion (by a separate adhesive layer G09F3/10) · CPC title
comprising polyolefins {(comprising vinyl (co)polymers or acrylic (co)polymers B32B27/30)} · CPC title
using multilayered plates or sheets · CPC title
characterised by the choice of materials · CPC title
Related publications grouped by family.
Answers are generated from the same data shown on this page.